Table 2. Magnetic characteristics of SCPFe composite

Sample Ms (emu/g) Mr (emu/g) Mc (Oe)
SCPFe0 0.00 0 0
SCPFe10 0.01 0.063 99.40
SCPFe20 0.02 0.114 87.50
SCPFe30 0.04 0.175 239.16
SCP: sawdust cellulose powder, Ms: saturation magnetization, Mr: remanent magnetization, Mc: magnetic coercivity.