Table 6. Weight loss of treated wood due to subterranean termites in field tests

Groups Treatment Weight loss (g)
A0 Nanocellulose (control) 429.62a ± 1.97
A1 Nanocellulose 20% and Metarhizium anisopliae 367.10b ± 1.55
A2 Nanocellulose 40% and M. anisopliae 363.61c ± 1.73
A3 Nanocellulose 60% and M. anisopliae 308.17d ± 1.46
B1 Nanocellulose 20% and Beauveria bassiana 373.84e ± 0.63
B2 Nanocellulose 40% and B. bassiana 347.72f ± 1.74
B3 Nanocellulose 60% and B. bassiana 326.45g ± 1.89
C1 Nanocellulose 20% and Trichoderma harzianum 435.14h ± 1.16
C2 Nanocellulose 40% and T. harzianum 364.94i ± 1.83
C3 Nanocellulose 60% and T. harzianum 318.71j ± 1.72
Different letter ranks indicate a significant difference between treatments.