Table 5. Weight loss of treated wood exposed to subterranean termites

Groups Treatment Weight loss (g)
A0 Nanocellulose (control) 2.528a ± 0.21
A1 Nanocellulose 20% and Metarhizium anisopliae 1.510b ± 0.15
A2 Nanocellulose 40% and M. anisopliae 1.060c ± 0.24
A3 Nanocellulose 60% and M. anisopliae 0.708d ± 0.12
B1 Nanocellulose 20% and Beauveria bassiana 1.48c ± 0.16
B2 Nanocellulose 40% and B. bassiana 1.13d ± 0.18
B3 Nanocellulose 60% and B. bassiana 0.91e ± 0.18
C1 Nanocellulose 20% and Trichoderma harzianum 4.95h ± 0.14
C2 Nanocellulose 40% and T. harzianum 5.74i ± 0.14
C3 Nanocellulose 60% and T. harzianum 6.64j ± 0.11
Different letter ranks indicate a significant difference between treatments.