Table 3. Deodorization rate of ceramics prepared at different mixing ratio of sawdust, rice husk and charcoal

Mixing ratio of sawdust:rice husk:charcoal (%) Running time (min) Concentration of blank (μmol/mol) Concentration of sample (μmol/mol) Deodorization rate (%)
50:35:05 0 20 20
30 20 4 80
60 20 3 85
90 20 3 85
120 20 3 85
50:30:10 0 20 20
30 20 3.8 81
60 20 2.8 86
90 20 2.8 86
120 20 2.6 87
50:25:15 0 20 20
30 20 3.8 81
60 20 2.8 86
90 20 2.4 88
120 20 2.4 88
50:20:20 0 20 20
30 20 3.6 82
60 20 2.4 88
90 20 2.4 88
120 20 2.2 89