Table 4.
The ANOVA summary of the pulping data

Response Factors
Active alkali (A) L/W ratio (B) Interaction of A and B
Kappa number 0.000** 0.014* 0.000**
Degree of delignification 0.000** 0.014* 0.000**
Klason lignin 0.000** 0.015* 0.000**
Delignification selectivity 0.000** 0.000** 0.000**
Pulping yield 0.000** 0.000** 0.000**
Note: : significant and