Table 1.
Composition of MEG and nano SiO
2
solutions used for impregnation.
Treatment
MEG (mL)
Water (mL)
Nano SiO
2
(g)
Untreated
0
1000
0
MEG
500
500
0
0.5% MEGSiO
2
500
500
5