Table 4.
Shrinkage of wood produced in each province
Province&Condition | Goseong-gun | Hongcheon-gun | Bonghwa-gun |
Position | Air dry | Oven dry | Air dry | Oven dry | Air dry | Oven dry |
Tangential(%) | 2.86 B* ±1.45 | 6.32 b ±2.94 | 3.94 A ±0.79 | 6.58 b ±1.28 | 4.39 A ±0.86 | 9.85 a ±4.12 |
Radial(%) | 1.73 A ±0.81 | 2.83 a ±0.90 | 2.09 A ±0.92 | 3.44 a ±1.40 | 2.29 A ±0.63 | 3.68 a ±0.52 |
T/R | 1.67 | 2.11 | 1.89 | 1.04 | 1.92 | 2.68 |
The same letters indicate no significant difference by Duncan's multiple test at 0.05 level. Air dry = Capital letter, Oven dry = Small letter.